Information sources:本站 | Release date: 2020-02-27 16:06:14 | Browse volume:15543
(8) Cracks and cracks ◇ Excessive demoulding, the impact of external force on the surface of the gel coat.◇ The gel coat is too thick and the exothermic temperature is high.◇ The impact force inside the structural layer causes spider web-like cr…
(8) Cracks and cracks
◇ Excessive demoulding, the impact of external force on the surface of the gel coat.
◇ The gel coat is too thick and the exothermic temperature is high.
◇ The impact force inside the structural layer causes spider web-like cracks on the surface of the gel coat.
◇ There are cracks on the mold surface.
◇ The structural layer has insufficient rigidity and insufficient curing.
◇ Poor adhesion between gel coat layer and structural layer.
When you make a product, each ingredient is carefully selected, and this level of attention should also be given when you choose a refrigerat…
(1) Gel coat wrinkles Wrinkles are mainly caused by uneven curing of the gel coat, and there are many factors that cause uneven curing, s…
FRP pipes are mainly used in petroleum, chemical, electric power, metallurgy, medicine and other fields. They are light in weight, high in st…
(2) Exposed fiber◇ If the gel coat is thin and the gel coat is not cured completely, the reinforcement layer is applied.◇ The fiber rolling…